33% Carbon-Fiber-Filled Nylon 12 optimized for a smooth surface finish without sacrificing feature details. Highlights: - High-Detail Black Surface Finish
- Good Stiffness and Mechanical Properties
- Warping Resistance at Elevated Temperatures
Applications: - High-performance impact sports equipment and racing applications
- Industrial applications with an HDT of ~177° C
- Wind tunnel model testing
Information provided by Advanced Laser Materials |