MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

American Elements Molybdenum Nanoparticles
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: General Description

Molybdenum (Mo) Nanoparticles, nanodots or nanopowder are black high surface area particles. Nanoscale Molybdenum Particles are typically 50 - 100 nanometers (nm) with specific surface area (SSA) in the 1 – 5 m 2 /g range. Nano Molybdenum Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for molybdenum nanocrystals include as a high surface area catalyst and catalyst support and as the catalysts in the synthesis of vertically aligned carbon nanotubes and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications.

Key Words: Formula: Mo; CAS Number: 7439-98-7
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.28 g/cc0.3714 lb/in³
Particle Size 0.050 - 0.10 µm0.050 - 0.10 µm
Specific Surface Area 1.0 - 5.0 m²/g1.0 - 5.0 m²/g
Molecular Weight 95.94 g/mol95.94 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 2623 °C4753 °F
Boiling Point 4639 °C8382 °F
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Molybdenum Disilicide, MoSi2
HWM-25 Molybdenum Alloy
AISI 4130 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
Zircar Ceramics MOSI2 Molybdenum Disilicide Heating Element
W-50Mo Tungsten Alloy

EJAMER56 / 5539

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.