MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Westlake Epolene® C-16P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: Epolene C-16P is a branched low density polyethylene powder modified with maleic anhydride. It is useful as a base polymer for adhesives and coatings, color concentrate dispersions, and applications requiring compatibility with polyamide. Coatings produced with Epolene C-16P exhibit high gloss, low moisture vapor transmission rates, grease resistance, and good heat-seal ability. In hot melt adhesives, the maleic anhydride modification allows for improved adhesion, greater filler tolerance, broader capabilities, and improved aging properties.
    Key Attributes:
  • Enhances paraffin wax coating properties like gloss, grease resistance, and MVTR
  • Excellent thermal stability
  • Maleic anhydride grafted PE provides functionality
  • Medium molecular weight
  • Useful in color concentrates
    Application/Uses:
  • Automotive
  • Building and Construction
  • Hot Melt Adhesives
  • Packaging
  • Solvent borne Adhesives
  • Wax Modification

    Information provided by Westlake Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 - 0.920 g/cc0.890 - 0.920 g/cc
Viscosity 6300 - 10000 cP
@Temperature 150 °C
6300 - 10000 cP
@Temperature 302 °F
542-111
Brookfield Viscosity  2850 cP
@Temperature 190 °C
2850 cP
@Temperature 374 °F
 16650 cP
@Temperature 125 °C
16650 cP
@Temperature 257 °F
Molecular Weight 26000 g/mol26000 g/mol
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 2.02.0mg KOH/g
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 261 °C>= 502 °F
Ring & Ball Softening Point 102 °C216 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 1.0<= 1.0542-130
 
Descriptive Properties
Penetration Hardness3 dmmASTM D5, Needle under 100-g load for 5s @ 25 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Epolene® E-43P Oxidized Low Molecular Weight Polyethylene Polymer
Honeywell A-C® 8 Low Density PE homopolymer
Honeywell A-C® 7 Low Density PE homopolymer
Honeywell A-C® 617A PE homopolymer
Honeywell A-C® 6 Low Density PE homopolymer

PWESF8904 / 133449

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.