MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 50% Glass Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% and 54% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.67 - 1.88 g/cc0.0603 - 0.0679 lb/in³Average value: 1.72 g/cc Grade Count:36
 1.44 - 1.56 g/cc
@Temperature 245 - 285 °C
0.0520 - 0.0564 lb/in³
@Temperature 473 - 545 °F
Average value: 1.50 g/cc Grade Count:2
Filler Content 45.0 - 50.0 %45.0 - 50.0 %Average value: 46.0 % Grade Count:5
Water Absorption 0.0350 - 0.620 %0.0350 - 0.620 %Average value: 0.171 % Grade Count:14
Moisture Absorption at Equilibrium 0.120 - 0.210 %0.120 - 0.210 %Average value: 0.157 % Grade Count:8
Viscosity  15000 - 300000 cP
@Temperature 270 - 315 °C
15000 - 300000 cP
@Temperature 518 - 599 °F
Average value: 133000 cP Grade Count:2
 15000 - 300000 cP
@Shear Rate 1000 - 100000 1/s
15000 - 300000 cP
@Shear Rate 1000 - 100000 1/s
Average value: 133000 cP Grade Count:2
Viscosity Number 55.0 - 60.0 cm³/g0.550 - 0.600 dl/gAverage value: 57.0 cm³/g Grade Count:4
Linear Mold Shrinkage 0.000500 - 0.00900 cm/cm0.000500 - 0.00900 in/inAverage value: 0.00266 cm/cm Grade Count:28
 0.00250 - 0.00250 cm/cm
@Temperature 275 - 275 °C
0.00250 - 0.00250 in/in
@Temperature 527 - 527 °F
Average value: 0.00250 cm/cm Grade Count:2
 0.00250 - 0.00250 cm/cm
@Pressure 60.0 - 60.0 MPa
0.00250 - 0.00250 in/in
@Pressure 8700 - 8700 psi
Average value: 0.00250 cm/cm Grade Count:2
Linear Mold Shrinkage, Transverse 0.00200 - 0.0100 cm/cm0.00200 - 0.0100 in/inAverage value: 0.00688 cm/cm Grade Count:15
 0.0100 - 0.0100 cm/cm
@Temperature 275 - 275 °C
0.0100 - 0.0100 in/in
@Temperature 527 - 527 °F
Average value: 0.0100 cm/cm Grade Count:2
 0.0100 - 0.0100 cm/cm
@Pressure 60.0 - 60.0 MPa
0.0100 - 0.0100 in/in
@Pressure 8700 - 8700 psi
Average value: 0.0100 cm/cm Grade Count:2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100 - 125100 - 125Average value: 118 Grade Count:5
Hardness, Rockwell R 116 - 121116 - 121Average value: 119 Grade Count:7
Tensile Strength, Ultimate 129 - 210 MPa18700 - 30500 psiAverage value: 176 MPa Grade Count:26
Tensile Strength, Yield 0.866 - 195 MPa126 - 28300 psiAverage value: 142 MPa Grade Count:10
Elongation at Break 1.00 - 6.00 %1.00 - 6.00 %Average value: 2.16 % Grade Count:31
Modulus of Elasticity 12.6 - 19.0 GPa1830 - 2760 ksiAverage value: 16.7 GPa Grade Count:19
Flexural Yield Strength 177 - 300 MPa25600 - 43500 psiAverage value: 261 MPa Grade Count:21
 110 - 370 MPa
@Temperature -40.0 - 120 °C
16000 - 53700 psi
@Temperature -40.0 - 248 °F
Average value: 240 MPa Grade Count:1
Flexural Modulus 9.32 - 17.0 GPa1350 - 2470 ksiAverage value: 13.8 GPa Grade Count:25
 4.69 - 4.69 GPa
@Temperature 120 - 120 °C
680 - 680 ksi
@Temperature 248 - 248 °F
Average value: 4.69 GPa Grade Count:1
Poissons Ratio 0.3300.330Average value: 0.330 Grade Count:5
Izod Impact, Notched 0.694 - 1.15 J/cm1.30 - 2.15 ft-lb/inAverage value: 0.948 J/cm Grade Count:19
 0.900 - 0.900 J/cm
@Temperature -20.0 - -20.0 °C
1.69 - 1.69 ft-lb/in
@Temperature -4.00 - -4.00 °F
Average value: 0.900 J/cm Grade Count:1
Izod Impact, Unnotched 0.932 - 9.60 J/cm1.75 - 18.0 ft-lb/inAverage value: 6.00 J/cm Grade Count:3
Izod Impact, Notched (ISO) 9.50 - 13.0 kJ/m²4.52 - 6.19 ft-lb/in²Average value: 10.7 kJ/m² Grade Count:5
 9.00 - 9.00 kJ/m²
@Temperature -30.0 - -30.0 °C
4.28 - 4.28 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 9.00 kJ/m² Grade Count:2
Charpy Impact Unnotched 2.40 - 6.50 J/cm²11.4 - 30.9 ft-lb/in²Average value: 5.06 J/cm² Grade Count:13
 2.10 - 6.50 J/cm²
@Temperature -30.0 - -30.0 °C
9.99 - 30.9 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 4.44 J/cm² Grade Count:9
Charpy Impact, Notched 0.770 - 1.40 J/cm²3.66 - 6.66 ft-lb/in²Average value: 1.06 J/cm² Grade Count:17
 0.900 - 1.40 J/cm²
@Temperature -30.0 - -30.0 °C
4.28 - 6.66 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 1.07 J/cm² Grade Count:9
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 - 4.00e+16 ohm-cm1.00e+13 - 4.00e+16 ohm-cmAverage value: 6.15e+15 ohm-cm Grade Count:20
Surface Resistance 1.00e+13 - 1.00e+15 ohm1.00e+13 - 1.00e+15 ohmAverage value: 3.92e+14 ohm Grade Count:12
Dielectric Constant 3.40 - 5.203.40 - 5.20Average value: 4.11 Grade Count:15
Dielectric Strength 15.0 - 35.0 kV/mm381 - 889 kV/inAverage value: 25.7 kV/mm Grade Count:16
Dissipation Factor 0.00200 - 0.2200.00200 - 0.220Average value: 0.0207 Grade Count:11
Arc Resistance 120 - 129 sec120 - 129 secAverage value: 125 sec Grade Count:3
Comparative Tracking Index 175 - 399 V175 - 399 VAverage value: 253 V Grade Count:13
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.0 - 30.0 µm/m-°C5.56 - 16.7 µin/in-°FAverage value: 19.0 µm/m-°C Grade Count:15
CTE, linear, Transverse to Flow 35.0 - 100 µm/m-°C19.4 - 55.6 µin/in-°FAverage value: 66.4 µm/m-°C Grade Count:8
Melting Point 240 - 260 °C464 - 500 °FAverage value: 249 °C Grade Count:21
Maximum Service Temperature, Air 75.0 - 140 °C167 - 284 °FAverage value: 96.7 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 226 - 255 °C439 - 491 °FAverage value: 245 °C Grade Count:18
Deflection Temperature at 1.8 MPa (264 psi) 204 - 242 °C400 - 468 °FAverage value: 228 °C Grade Count:32
Deflection Temperature at 8.0 MPa 145 - 180 °C293 - 356 °FAverage value: 164 °C Grade Count:4
Vicat Softening Point 230 - 260 °C446 - 500 °FAverage value: 246 °C Grade Count:5
Glass Transition Temp, Tg 73.0 - 95.0 °C163 - 203 °FAverage value: 88.0 °C Grade Count:6
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:29
Oxygen Index 20.0 - 26.0 %20.0 - 26.0 %Average value: 22.5 % Grade Count:4
Glow Wire Test 750 - 900 °C1380 - 1650 °FAverage value: 832 °C Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 110 - 300 °C230 - 572 °FAverage value: 237 °C Grade Count:5
Melt Temperature 240 - 300 °C464 - 572 °FAverage value: 279 °C Grade Count:13
Mold Temperature 40.0 - 149 °C104 - 300 °FAverage value: 114 °C Grade Count:16
Drying Temperature 120 - 140 °C248 - 284 °FAverage value: 126 °C Grade Count:13
Moisture Content 0.0100 - 0.0800 %0.0100 - 0.0800 %Average value: 0.0280 % Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

O3315 / 78201

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.