MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Von Roll Dellit® 2063 V0 Phenolic - Paper Laminate
Categories: Polymer; Thermoset; Phenolic

Material Notes: Canevasite® is a range of phenolic cotton laminates comprises several grades, each having specific properties and most of which are remarkable for their abrasion resistance and wear properties as well as good level of flexibility and very low level of water absorption. Machined parts made from Canevasite® substantially extend the life of machines and mechanically stressed components, thereby resulting in excellent cost savings. The Dellit® range encompasses a group of cellulose paper-based laminates that are either phenolic- or epoxy-bonded. All of these laminates comply with precise standards and/or specific requirements such as flame retardancy or high-tension resistance. Besides the well-known standard grades, we offer several special grades. Highlight:

Information provided by Von Roll.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Water Absorption 0.65 %0.65 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 70.0 MPa10200 psiISO 527
Flexural Strength 120 MPa
@Temperature 23.0 °C
17400 psi
@Temperature 73.4 °F
flatwise; ISO 178
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²Edgewise; ISO 179
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+17 ohm1.00e+17 ohmafter immersion in water; IEC 60167
Dielectric Strength 10.0 kV/mm254 kV/inflatwise; IEC 60243-1
Dielectric Breakdown 35000 V35000 VTaper pin electrodes, edgewise; IEC 60243-1
Comparative Tracking Index 200 V200 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C11.1 µin/in-°FDIN 53752
Maximum Service Temperature, Air 105 °C221 °FTemperature Index; IEC 60216
 
Descriptive Properties
ColorLight brown
ReinforcementPaper
Sheet Size (mm)1170 x 1070

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVONR9944 / 249234

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.