MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Thermal Ceramics Superwool 607 Blanket
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Superwool is designed from pure raw materials and specially processed to offer excellent performance in high temperature applications. Superwool offers an alternative to traditional solutions due to its exceptional properties of high refractoriness and excellent non-wetting characteristics in applications requiring direct contact with molten aluminum.

Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalis (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying.

Although Superwool’s basic fiber form offers an economical alternative for most applications, they can be engineered to meet the requirements of specific applications. Fiber diameter, shot content, fiber length and form can be altered as required to achieve desired properties for specific applications.

Features:

  • Low biopersistence
  • Thermal stability
  • Low heat storage
  • Good resistance to tearing
  • Flexible and resilient
  • Immune to thermal shock
  • Excellent thermal insulating performance
  • Based on patented technology
  • Applications

  • Expansion joints construction
  • Base seals
  • Low mass kiln car construction
  • Tube seal fabrication
  • Thermal and acoustical insulation
  • As primary raw material for high temperature converted and engineering fibers - Enfil®
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.0640 g/cc0.00231 lb/in³Available in multiple densities
     0.0960 g/cc0.00347 lb/in³Available in multiple densities
     0.128 g/cc0.00462 lb/in³Available in multiple densities
     0.160 g/cc0.00578 lb/in³Available in multiple densities
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0605 W/m-K
    @Temperature 260 °C
    0.420 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    8 pcf; ASTM C201
     0.0663 W/m-K
    @Temperature 260 °C
    0.460 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    6 pcf; ASTM C201
     0.127 W/m-K
    @Temperature 538 °C
    0.880 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    8 pcf; ASTM C201
     0.147 W/m-K
    @Temperature 538 °C
    1.02 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    6 pcf; ASTM C201
     0.220 W/m-K
    @Temperature 816 °C
    1.53 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    8 pcf; ASTM C201
     0.256 W/m-K
    @Temperature 816 °C
    1.78 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    6 pcf; ASTM C201
     0.281 W/m-K
    @Temperature 982 °C
    1.95 BTU-in/hr-ft²-°F
    @Temperature 1800 °F
    8 pcf; ASTM C201
     0.329 W/m-K
    @Temperature 982 °C
    2.28 BTU-in/hr-ft²-°F
    @Temperature 1800 °F
    6 pcf; ASTM C201
    Melting Point 1470 °C2680 °F
    Maximum Service Temperature, Air 1000 °C1832 °F
    Shrinkage  2.0 %
    @Temperature 538 °C,
    Time 86400 sec
    2.0 %
    @Temperature 1000 °F,
    Time 24.0 hour
     3.0 %
    @Temperature 982 °C,
    Time 86400 sec
    3.0 %
    @Temperature 1800 °F,
    Time 24.0 hour
     
    Component Elements PropertiesMetricEnglishComments
    CaO 25 - 35 %25 - 35 %
    MgO 4.0 - 7.0 %4.0 - 7.0 %
    SiO2 60 - 70 %60 - 70 %
     
    Descriptive Properties
    Alumina Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Unifrax PC Series™ PC Max™ Paper Ceramic Fiber Filtration Media
    Pyrotek Grade 1250 Ceramic fiber paper
    Morgan Advanced Ceramics Thermo-Bloc Modules Ceramic Fiber Thermal Ceramic
    Morgan Advanced Ceramics Pyro-Bloc® Module HS Thermal Ceramic
    Morgan Advanced Ceramics Pyro-Bloc® EES System R Thermal Ceramic

    CTHERM286 / 2606

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.