Evonik VESTAGON® B 1065 Colorant
Categories:
Other Engineering Material
;
Additive/Filler for Polymer
;
Polymer
;
Thermoset
Material Notes:
VESTAGON® B 1065 is a polyisocyanate adduct used in combination with hydroxyl functional resins. Due to the e-Caprolactam blocked NCO-groups it is stable during processing up to the unblocking temperature of more than 170°C.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.670
g/cc
0.0242
lb/in³
DIN 53 466
Density
1.15
g/cc
0.0415
lb/in³
DIN 53 479
Thermal Properties
Metric
English
Comments
Melting Point
59.0
-
79.0
°C
138
-
174
°F
DIN 53 736
Glass Transition Temp, Tg
43.0
-
54.0
°C
109
-
129
°F
DSC
Flash Point
200
°C
392
°F
ISO 2592
Ignition Temperature
420
°C
788
°F
DIN 51 794
Descriptive Properties
NCO content (% wt)
<1
DIN EN ISO 11 909; free
10.1-10.8
DIN EN ISO 11 909; total
NCO-equivalent (g/Eq)
400
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
AISI 1065 Steel, cold drawn, spheroidized, annealed, 19-32 mm (0.75-1.25 in) round
AISI 1065 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1566 Steel Composition Spec (UNS G15660)
AISI 1064 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1064 Steel, cold drawn, spheroidized, annealed, 19-32 mm (0.75-1.25 in) round
PHUMB378 / 81380
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.