MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem ANOX™ 1315
Categories: Other Engineering Material

Material Notes: Product Description: ANOX™ 1315 stabilizer is a highly effective, very low emissive, non-discoloring, liquid hindered phenolic antioxidant. It is an efficient antioxidant for any kind of polymer providing very good protection against degradation due to heat and oxygen.
  • Excellent antioxidant for polymers (ie. PVC, PE, ABS, SBR, BR, and NBR)
  • Excellent antioxidant for lubricating oils, both engine and cutting.
  • For use in polyether and polyester polyols for polyurethane foams for storage and scorch protection because of its efficiency and favorable low volatility. It can be used for a variety of applications in the coating, furniture, bedding and automotive industry where strict emission regulations are applied. It can be added with additional antioxidants and/or co-stabilizers and/or light stabilizers.

    Features:

    • Easy to handle low-viscosity liquid antioxidant.
    • Great compatibility and solubility to various substrates, rendering the product highly flexible in its uses.
    • Liquid even at temperatures blow freezing point
    CAS Number: 171090-93-0

    Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/cc
Viscosity 360 - 400 cP360 - 400 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 178 °C352 °F
 
Descriptive Properties
AppearanceViscous, clear yellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH474 / 315392

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.