System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Total 5502 BZ HDPE injection blow molding
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Blow Molding Grade
Material Notes:
Applications: Cosmetics and toiletries, pharmaceuticals, specialty containers, food packaging
Information provided provided by Total Petrochemicals.
Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.955
g/cc
ASTM D 792
Environmental Stress Crack Resistance
35
hour
ASTM D1693 cond. B 10% lgepal
50
hour
ASTM D1693 cond. B 100% lgepal
Melt Flow
0.35
g/10 min
@Load 2.16 kg
ASTM D 1238
High Load Melt Index
30
g/10 min
@Load 21.6 kg
ASTM D 1238
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
4000
psi
ASTM D 638 type IV
Elongation at Break
>= 600 %
ASTM D 638 type IV
Flexural Modulus
200000
psi
ASTM D 790
Thermal Properties
Original Value
Comments
Melting Point
264
°F
ASTM D3417
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
Total 5502 R3 High Density Polyethylene - Blow Molding
SIDPEC EGYPTENE® HD 5502 GA HDPE Blow Molding
Chevron Phillips Marlex® 9503H HDPE Blow Molding Resin
Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE
PFINAP144 / 38727
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.