MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

MRC Polymers MAXTEL 600T30IM Thermoplastic olefin
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: MAXTEL 600T30IM is 30% talc filled high impact TPO. This material is available in black. It can be color matched black and either UV or non-UV stable. It is typically used for automotive interior/exterior applications.

Information provided by MCR Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccISO 1183
Filler Content 30 %30 %ISO 3451
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 16.0 MPa2320 psiISO 527
Flexural Strength 23.0 MPa3340 psiISO 178
Flexural Modulus 1.40 GPa203 ksiISO 178
Charpy Impact, Notched 6.80 J/cm²32.4 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C126 °Funannealed; ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMRC5025 / 217611

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.