Use: Addocat LTB may be used as accelerator for epoxy/hardener- combinations and for the catalytic curing of epoxy resins due to its excellent hydrolysis stability as well as good activity. In case of epoxy/hardener- combinations, e.g. 100 pbw epoxy and 32 pbw hardener and 1.0 pbw Addocat LTB, at 160 °C a gel time of 5 to 10 minutes is reached; by 3.0 pbw Addocat LTB, at 160 °C a gel time of 3 minutes can be expected.. Function: Accelerator for epoxy/hardener-combinations and for the catalytic curing of epoxy resins. Information provided by Lanxess. |