MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kennametal Stellite Stoody® 12 Cobalt-Base Cast Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Stood® 12 is a high carbon, chromium, tungsten, cobalt-base centrifugally cast alloy designed to have intermediate properties between Stood 1 and Stood 6. Being a compromise between Alloys 1 and 6, it has intermediate wear resistance. With minor modifications, Stood 12 can be manufactured to conform to MIL-C-24248 (ship), Composition II.

Recommended for twist rolls, shaft sleeves, bushings, glider knives.

Information provided by Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Key Words: MIL-C-24248
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 48 - 5248 - 52
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.5 %1.5 %
Chromium, Cr 29.5 %29.5 %
Cobalt, Co 56 %56 %As remainder
Iron, Fe 1.0 %1.0 %
Nickel, Ni 1.0 %1.0 %
Other 1.5 %1.5 %
Silicon, Si 1.0 %1.0 %
Tungsten, W 8.5 %8.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 21
Kennametal Stellite Stoody® 6 Cobalt-Base Cast Alloy
Kennametal Stellite Stellite® 6 PM with P/M Processing
Kennametal Stellite Stellite® 12 PM with P/M Processing
Kennametal Stellite Stoody® 1 Cobalt-Base Cast Alloy

NSST12 / 19203

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.