MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics Ultra Ethylux® HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Ultra Ethylux® High Density Polyethylene (HDPE) is one of the most widely utilized thermoplastics due to its relative low cost, light weight, toughness, resistance to a broad range of chemicals and low moisture absorption. It meets a range of regulatory standards making it suitable for use in food processing, medical device and pharmaceutical processing and packaging applications.

Industry: Chemical Process; Engineering; Semiconductor and ESD

Colors Available: Natural

Attributes: Chemical Resistance

Shapes: Compression Sheet; Extruded Sheet; Extruded Film

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4600 psiASTM D638
Elongation at Break >= 400 %ASTM D638
Flexural Modulus 225000 psi1% Secant; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 180 °FASTM D648
 
Descriptive Properties
ColorNatural-Translucent White, Grey, Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
LyondellBasell Alathon® M6080 High Density Polyethylene, Injection Molding Grade
NOVA Chemicals Sclair® 58A/58A-DE3 HDPE Blow Molding Resin
Borealis BL2571 High Density Polyethylene

PWEST148 / 72767

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.