MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Oxygen (O2)
Categories: Fluid; Pure Element

Material Notes: Physical Form: Colorless Gas

Key Words: O2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.001308 g/ccGas
Molecular Weight 31.999 g/mol
Vapor Pressure 0.09869 atm
@Temperature -200.5 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 15.99941995
Atomic Number 8
X-ray Absorption Edge 23.301 ÅK
Critical Pressure 49.77 atm
Critical Temperature -118.56 °C
 427.75 °C
Critical Density 0.438 g/cc
Critical Molar Volume 73.0 cm³/mol
Electronegativity 3.44Pauling
Ionic Radius 0.0900 ÅCrystal Ionic Radius for Valence +6
 0.220 ÅCrystal Ionic Radius for Valence +1
 1.32 ÅCrystal Ionic Radius for Valence -2
 1.76 ÅCrystal Ionic Radius for Valence -1
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.507
@Temperature -193 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 13.8 J/gEnthalpy of fusion at normal melting point
Heat of Vaporization 213.1 J/gEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 0.918 J/g-°C
Thermal Conductivity 0.00930 W/m-K
@Pressure 0.100 MPa,
Temperature -173 °C
gas
 0.0184 W/m-K
@Pressure 0.100 MPa,
Temperature -73.1 °C
gas
 0.0263 W/m-K
@Pressure 0.100 MPa,
Temperature 26.9 °C
gas
 0.0337 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
gas
 0.0410 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
gas
 0.0481 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
gas
Melting Point -218.79 °CAt atmospheric pressure (760 torr)
Boiling Point -182.95 °C
Heat of Formation 0.000 kJ/molGas
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.2243
@Temperature -183 °C,
Wavelength 546 nm
 
Component Elements PropertiesOriginal ValueComments
Oxygen, O 100 %
 
Descriptive Properties
AppearanceColorless Gas
CAS Number7782-44-7
SolubilitySlightly Soluble in H2O, EtOH and Organic Solvents

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hydrogen, H2
Argon, Ar
Nitrogen, N2
Helium, He
Neon, Ne

AMEO0 / 74

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.