MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kuraray Genestar™ TA104 Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Reinforced injection grade.

Main Features:

  • High reflectivity
  • Less color change by heat and light
  • High reliability

Example of applications:

  • LED reflectors

Key Words: PA9T
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.61 g/cc1.61 g/cc
Linear Mold Shrinkage, Flow 0.012 cm/cm
@Thickness 1.00 mm
0.012 in/in
@Thickness 0.0394 in
Linear Mold Shrinkage, Transverse 0.011 cm/cm
@Thickness 1.00 mm
0.011 in/in
@Thickness 0.0394 in
Spiral Flow 5.40 cm
@Load 750 kg,
Temperature 320 °C
2.13 in
@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psiASTM D638
Elongation at Break 1.4 %1.4 %
Flexural Strength 83.0 MPa12000 psiASTM D790
Flexural Modulus 4.50 GPa653 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 192 °C378 °FASTM D648
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Descriptive Properties
ApplicationsLED Reflectors
Other FeaturesHigh reflectivity
 High reliabaility
 Less color change by heat and light

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kuraray Genestar™ GC1201A-M41 Nylon, Glass Filled and Carbon Filled
Kuraray Genestar™ N1000A-M41 Nylon
Kuraray Genestar™ N1006A-M41 Nylon
Kuraray Genestar™ N1001A-M41 Nylon
Kuraray Genestar™ N1001D-U03 Nylon

PKUR115 / 162504

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.