MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Entec Ezprene® 9030A TPV
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Product Description: 30 Shore A TPE (Thermoplastic Vulcanizate). Available in black, natural or pre-colored for injection molding and extrusion applications. This ultra-soft, easy to color material is non-hydroscopic and offers excellent chemical resistance and physical properties. EZPrene is polyolefin based and is 100% recyclable.

Availability: North America

Features: Chemical Resistant; Fatigue Resistant; Good Adhesion; Good Colorability; Low to No Water Absorption; Ozone Resistant; Recyclable Material; Soft; UV Resistant

Appearance: Black; Colors Available; Natural Color

Processing Method: Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.922 g/cc0.0333 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  31
@Time 5.00 sec
31
@Time 0.00139 hour
Extruded; ASTM D2240
 33
@Time 5.00 sec
33
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 3.70 MPa537 psiASTM D412
Tensile Stress 1.30 MPa
@Strain 100 %
189 psi
@Strain 100 %
ASTM D412
Elongation at Break 600 %600 %ASTM D412
Tear Strength 9.71 kN/m55.4 pliASTM D624
Compression Set  30 %
@Temperature 22.8 °C,
Time 79200 sec
30 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
 36 %
@Temperature 125 °C,
Time 252000 sec
36 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -70.0 °C-94.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 166 - 177 °C330 - 350 °FHopper, Extrusion
Rear Barrel Temperature 191 - 204 °C375 - 400 °F
Middle Barrel Temperature 196 - 210 °C385 - 410 °F
Front Barrel Temperature 196 - 210 °C385 - 410 °F
Nozzle Temperature 210 - 221 °C410 - 430 °F
Zone 1 171 - 191 °C340 - 375 °F
Zone 2 171 - 191 °C340 - 375 °F
Zone 3 171 - 191 °C340 - 375 °F
Zone 4 171 - 191 °C340 - 375 °F
Zone 5 171 - 191 °C340 - 375 °F
Adapter Temperature 191 - 210 °C375 - 410 °F
Die Temperature 191 - 210 °C375 - 410 °F
Melt Temperature 191 - 199 °C375 - 390 °FExtrusion
 199 - 221 °C390 - 430 °FInjection
Mold Temperature 23.9 - 51.7 °C75.0 - 125 °FInjection
Drying Temperature 82.2 °C180 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
Injection Pressure 5.17 - 8.96 MPa750 - 1300 psi
Cushion 0.508 - 1.27 cm0.200 - 0.500 in
Screw Speed 30 - 80 rpm30 - 80 rpmExtrusion
 50 - 200 rpm50 - 200 rpmInjection
 
Descriptive Properties
Dynamic Service Temperature266°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENTB672 / 311365

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.