MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Honeywell Genetron® 134a Refrigerant
Categories: Fluid

Material Notes: Genetron® 134a (1,1,1,2-tetrafluoroethane) is a non-ozonedepleting, environmentally safer refrigerant developed by Honeywell to replace CFCs and HCFCs in several air-conditioning and refrigeration applications. It possesses similar energy efficiency and capacity characteristics as CFC-12, has an intrinsically low toxicity, and is recognized as a superior long-term solution in many applications. This document is meant to provide engineers, technicians, and mechanics with basic Genetron 134a properties, plus application and handling information to facilitate safe and efficient usage.

Applications
Stationary Refrigeration and Air-Conditioning: Genetron 134a can be used in refrigeration applications including supermarket cases, walk-in coolers, beverage dispensers, vending machines, water coolers and home refrigerators. Genetron 134a is also used in centrifugal chillers. Genetron 134a is suitable for both new equipment and for retrofitting existing CFC-12 commercial refrigeration systems. Generally, there will be few equipment design changes necessary to optimize the performance of Genetron 134a in these applications. For further information on retrofitting, your Genetron refrigerants distributor or your Honeywell sales or technical representative can provide you with the most up-to-date retrofit literature. We also recommend consulting the original equipment manufacturer before performing any retrofit.
Automotive Air-Conditioning: Several automobile and truck manufacturers have selected Genetron 134a for the initial charge in their new vehicles. Additionally, retrofit kits for converting CFC-12 systems to Genetron 134a are widely available. Honeywell is also proud to offer Genetron 134aUV, a special formulation of Genetron 134a and a refrigerant-soluble dye that fluoresces when exposed to ultraviolet light. Genetron 134aUV was developed specifically for automotive mechanics who wanted a solution for making leak detection in cars and trucks easier, faster, and less expensive.
Aerosol and Foam-Blowing Applications: Genetron 134a is used as a propellant in many specialty aerosol products and may be used as a blowing agent for rigid-foam insulation. Additional information on the use of Genetron 134a in aerosol and foam applications is available through your Honeywell sales or technical representative.

Chemical Name 1,1,1,2-tetrafluoroethane

Molecular Formula CH2FCF3

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.00525 g/cc0.000190 lb/in³at Boiling Point
 0.51195 g/cc0.018494 lb/in³Critical
 1.207 g/cc0.04359 lb/in³Liquid
Volatiles 100 %100 %
Viscosity 11.7 cP11.7 cPVapor
 194.9 cP194.9 cPLiquid
Molecular Weight 102.03 g/mol102.03 g/mol
Vapor Pressure 0.00887 bar6.65 torr
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 40.59 bar30450 torr
Critical Temperature 101.06 °C213.91 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 217 J/g93.3 BTU/lbat Boiling Point
Specific Heat Capacity 1.43 J/g-°C0.341 BTU/lb-°FLiquid
 0.849 J/g-°C
@Pressure 0.101 MPa
0.203 BTU/lb-°F
@Pressure 14.7 psi
Vapor
Thermal Conductivity 13.8 W/m-K95.8 BTU-in/hr-ft²-°FVapor
 81.1 W/m-K563 BTU-in/hr-ft²-°FLiquid
Melting Point -96.61 °C
@Pressure 0.101 MPa
-141.9 °F
@Pressure 14.7 psi
Boiling Point -26.1 °C
@Pressure 0.101 MPa
-14.9 °F
@Pressure 14.7 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell Genetron® 404A Refrigerant
Solvay Chemicals SOLKANE® 134a Refrigerant
Solvay Chemicals SOLKANE® 410A
Ammonia, NH3
Syensqo (Solvay Specialty Polymers) Meforex® 134a Ozone-Friendly CFC Replacement

PHONWL131 / 179676

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.