MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Taiwan PU TPUI-ED64 General Polyester TPU Resin
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Key features:
  • Polyester base TPU material
  • Transparent pellet
  • Hardness: 65A-98A, 61D, 64D, 71D
  • Good wear and oil resistance
  • High abrasion resistance
  • Good performance on elongation
Application:
  • 1. Shoes Material: Shoe Soles, Shoes Decorations, Air Bag, Label, Oil Bag.
  • 2. Industrial Parts: Snow Boots, Buckle, Animal ID Tags, Mining Screens, O-ring.
  • 3. Wheel: Load Wheel, Skate Wheel, Trolley Wheel.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464
Tensile Strength 47.1 MPa6830 psi
Elongation at Break 450 %450 %
100% Modulus 20.6 MPa2990 psi
300% Modulus 30.4 MPa4410 psi
Resilience 2525[%], Impact
Abrasion 2020[mg]
 
Processing PropertiesMetricEnglishComments
Processing Temperature 200 °C392 °FCompression Zone
 210 °C410 °FMetering Zone
Feed Temperature 195 °C383 °F
Adapter Temperature 215 °C419 °F
Die Temperature 215 °C419 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU069 / 305799

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.