MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

BASF Ultramid® B3WG7 Nylon 6, 35% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: Ultramid B3WG7 is a 35% glass fiber reinforced injection molding PA6 grade for highly rigid, dimensionally stable components which are resistant to high temperature aging and have improved retention of properties in a hot water environment.

Applications: Typical applications include automotive clutch and accelerator pedals

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Moisture Absorption 2.00 %2.00 %50% RH; ISO 62
Water Absorption at Saturation 6.2 %6.2 %ISO 62
Melt Flow 45 g/10 min
@Load 5.00 kg,
Temperature 275 °C
45 g/10 min
@Load 11.0 lb,
Temperature 527 °F
Dry; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiConditioned; ISO 527
 195 MPa28300 psiDry; ISO 527
Elongation at Break  3.5 %
@Temperature 23.0 °C
3.5 %
@Temperature 73.4 °F
Dry; ISO 527
 3.8 %
@Temperature -40.0 °C
3.8 %
@Temperature -40.0 °F
Dry; ISO 527
 7.0 %
@Temperature 23.0 °C
7.0 %
@Temperature 73.4 °F
Conditioned; ISO 527
Tensile Modulus 7.20 GPa1040 ksiConditioned; ISO 527
 11.0 GPa1600 ksiDry; ISO 527
Flexural Modulus 10.0 GPa1450 ksiDry; ISO 178
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179
 11.0 J/cm²
@Temperature 23.0 °C
52.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179
 3.30 J/cm²
@Temperature 23.0 °C
15.7 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+13 ohm-cm1.00e+13 ohm-cmDry; IEC 60093
Dielectric Constant  3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
Dry; IEC 60250
 6.2
@Frequency 1e+6 Hz
6.2
@Frequency 1e+6 Hz
Conditioned; IEC 60250
Dissipation Factor  0.021
@Frequency 100 Hz
0.021
@Frequency 100 Hz
Dry; IEC 60250
 0.021
@Frequency 1e+6 Hz
0.021
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.19
@Frequency 100 Hz
0.19
@Frequency 100 Hz
Conditioned; IEC 60250
 0.19
@Frequency 1e+6 Hz
0.19
@Frequency 1e+6 Hz
Conditioned; IEC 60250
Comparative Tracking Index 450 V450 VConditioned; IEC 60112
 450 V450 VDry; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C10.0 µin/in-°F
CTE, linear, Transverse to Flow 65.0 µm/m-°C36.1 µin/in-°F
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FISO 75
UL RTI, Electrical  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL746B
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL746B
UL RTI, Mechanical with Impact  90.0 °C
@Thickness 1.50 mm
194 °F
@Thickness 0.0591 in
UL746B
 100 °C
@Thickness 3.00 mm
212 °F
@Thickness 0.118 in
UL746B
UL RTI, Mechanical without Impact  130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL746B
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL746B
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °F
Mold Temperature 80.0 - 90.0 °C176 - 194 °F
Drying Temperature 180 °C
@Time 7200 - 14400 sec
356 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8971 / 254929

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.