MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik VESTANAT® B 1370 Polyisocyanate
Categories: Polymer

Material Notes: VESTANAT B 1370 is a blocked, cycloaliphatic polyisocyanate for crosslinking of suitable hydroxylated resins, like polyester, acrylic and alkyd resins. It may be classified as an exceptionally light fast and weathering resistant resin. It is characterized by an excellent balance of reactivity and storage stability of the formulated paint.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc
@Temperature 25.0 °C
0.0372 lb/in³
@Temperature 77.0 °F
DIN 51 757
Solids Content 59 - 61 %59 - 61 %DIN EN/ISO 3251
Viscosity 2100 - 3100 cP
@Temperature 23.0 °C
2100 - 3100 cP
@Temperature 73.4 °F
DIN EN ISO 3219
Vapor Pressure 0.0100 bar
@Temperature 50.0 °C
7.50 torr
@Temperature 122 °F
 
Thermal PropertiesMetricEnglishComments
Flash Point 28.0 °C82.4 °Fclosed cup; DIN 53 213
 
Descriptive Properties
Hazen Color Index, max150DIN/ISO 6271
NCO content (% wt)<0.1DIN EN ISO 11 909; free
 <8DIN EN ISO 11 909; latent
Splitting Temperature (°C)130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHUMB395 / 81397

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.