MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ter Hell Plastic Terez® PC X 9005 GF 5 Polycarbonate, 5% Glass Fiber
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: Description: Polycarbonate, medium flowability, 5% glass fiber reinforced.

Application: For injection molded parts with increased demand of stiffness.

Information provided by Ter Hell Plastic GMBH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccISO 1183
Water Absorption 0.32 %ISO 62
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 60.0 MPadry; ISO 527
Tensile Strength, Yield 65.0 MPadry; ISO 527
Elongation at Break 20 %dry; ISO 527
Elongation at Yield 5.0 %dry; ISO 527
Tensile Modulus 3000 MPadry; ISO 527
Charpy Impact, Notched 10.0 kJ/m²dry; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75
Vicat Softening Point 135 °CB/50; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 300 °C
Drying Temperature 120 °C
Dry Time 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® F161 Epoxy Resin, 120 Glass Fabric
INEOS Styrolution Luran® S KR 2864C Colored ASA+PC
Tisan TISAKRIL® 15% Glass Fiber Reinforced ABS
Evonik VESTAMID® NRG 1003 PA 12
Evonik Trogamid® BX7304 Nylon Blend

PTERH907 / 120645

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.