MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Evonik VESTAMID® NRG 5901 BK Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: VESTAMID® NRG 5901 BK is a high molecular weight PA 12 material developed by Evonik. The performance characteristics make it a good choice for expanding the use of thermoplastic piping systems at higher operating pressures and larger diameters to replace metallic piping systems in a safe and cost effective manner. Besides extending the operating pressure limits of thermoplastic piping systems, VESTAMID® NRG 5901 BK offers many of the same benefits, and in most instances more superior performance, as conventional PE piping systems.
  • Tough and durable
  • Corrosion resistant
  • Resistant to heavy hydrocarbons
  • High resistance to Slow Crack Growth
  • Increased installation efficiencies
  • Reliable performance
These characteristics make the VESTAMID® NRG 5901 BK material a good choice when selecting appropriate thermoplastic piping materials in extending gathering and flow lines infrastructure. Besides extending the operating pressure limits of thermoplastic piping systems, VESTAMID® NRG 5901 BK offers many of the same benefits, and in most instances more superior performance, as conventional PE piping systems. The manufacturer recommends a processing temperature between 230°C (446°F) and 260°C (500°F) - in some cases up to 280°C (536°F) - during the injection molding and extrusion process. The mold temperature should be within a range of 60°C (140°F) to 100°C (212°F). Drying at 80°C (176°F) for 2 hours to 4 hours before processing is recommended. Polyamide 12 is a high performance thermo-plastic polymer with increased performance characteristics that translates into safe operations over the life of the installed line pipe. It has a considerable record of safe and proven experience in many demanding applications, including fuel lines in passenger cars, air brake tubing in trucks and off-shore applications. With its excellent UV resistance properties, NRG 5901 BK is well suited for long term outdoor applications. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.
Dry properties listed below
Industrial Sector: Energy, Oil and Gas
Processing: Injection molding, Extrusion
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Hydrolysis / hot water, UV / light / weathering, Wear / abrasion, Fatigue resistance, Oil / fuels
Additives: Unfilled
Applications: Corrosion protection, Tube and hose, Fittings
Processing: Profile extrusion, Pipe/Tube extrusion
Special Characteristics: U.V. stabilized, High viscosity
Features: Barrier properties, Low coefficient of friction, Lightweight, Weldable
Color: Black
Chemical Resistance: General chemical resistance

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³ISO 1183
Viscosity Number 203 cm³/g2.03 dl/gISO 307, 1157, 1628
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psiISO 527
Tensile Strength 40.0 MPa5800 psiISO 527
Tensile Stress 37.0 MPa
@Strain 50.0 %
5370 psi
@Strain 50.0 %
ISO 527
Tensile Strength, Yield 40.0 MPa5800 psiISO 527
Elongation at Break 127 %127 %Nominal; ISO 527
Elongation at Yield 11.0 %11.0 %ISO 527
Tensile Modulus 1.25 GPa181 ksiISO 527
Charpy Impact, Notched  1.80 J/cm²
@Temperature -40.0 °C
8.57 ft-lb/in²
@Temperature -40.0 °F
Type of failure: C; ISO 179/1eA
 2.30 J/cm²
@Temperature -30.0 °C
10.9 ft-lb/in²
@Temperature -22.0 °F
Type of failure: C; ISO 179/1eA
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
Type of failure: C; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 176 °C349 °FISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C109 °FISO 75-1/-2
Vicat Softening Point 132 °C
@Load 1.02 kg
270 °F
@Load 2.25 lb
50 K/h; ISO 306
Glass Transition Temp, Tg 36.0 °C96.8 °FISO 11357-1/-2
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7938 / 325070

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.