MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics WDS® Multiflex® HT Porextherm
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Engineered 3D flexible microporous insulation products offering extremely low and flat thermal conductivity values in a wide temperature range, hence providing outstanding insulating performances which are up to five times better than any other conventional insulator, together with excellent thermal tability up to 1050°C (1922°F). WDS® MultiFlex® uses WDS® Technology, which is the benchmark in microporous know-how: it is today the only available technology that allows to perfectly and consistently control and engineer both the texture and the distribution of the microporous mineral matrix ore in order to obtain superior thermal characteristics but with improved mechanical properties overall. WDS® MultiFlex® core is a composition of reinforced blend of opacified premium grade inorganic silicates available in different property formulations; this homogeneous mineral matrix is then covered with an outer envelope which may be either glass (ST grade) or stabilized amorphous silica (HT grade) cloths to enable fast and clean manipulation; the stitched grid guarantees the necessary flexibility and twisting properties. WDS® super-insulation is the definitive answer to any of your most demanding thermal insulation concerns when seeking for space and weight reduction together with effective energy savings in a very wide temperature spectrum. WDS® MultiFlex® complies with the standard specification for microporous insulation ASTM C1676. WDS® MultiFlex® products are non-flammable in accordance to DIN EN 13501-1, Euroclass

Information provided by Morgan Advanced Materials

Key Words: Porextherm
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 g/ccnominal
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 1.00 - 3.00 MParoom temperature; ASTM C165
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.250 BTU/lb-°F
@Temperature 400 °C
Thermal Conductivity 0.0280 W/m-K
@Temperature 200 °C
ASTM C177
 0.0350 W/m-K
@Temperature 400 °C
ASTM C177
 0.0430 W/m-K
@Temperature 600 °C
ASTM C177
 0.0600 W/m-K
@Temperature 800 °C
ASTM C177
Shrinkage 0.050 %
@Treatment Temp. 1000 °C
temperature applied to one side
 2.0 %
@Treatment Temp. 1000 °C
temperature applied to all side
 
Descriptive Properties
Classification Temperature (°C)1050
Textile Coveringamorphous silica

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6133 / 202917

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.