MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin NHP9023 Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ NHP9023 resin is a 15% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0 1.5mm and V1 at 0.75mm for thin-wall molding capability. NORYL NHP9023 is based on a unique co-polymer technology and exhibits good dimensional stability, high heat resistance, strong electrical performance, and very low specific gravity. It is an excellent candidate for copier fuser units, business equipment internal components, and electrical applications where thin-wall FR, modulus retention, and high heat resistance are required.

Features: Hydrolytic Stability,Low Creep Sensitivity,High Heat Resistance,Good Stiffness,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0500 %0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %0.20 %ISO 62-1
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 3.20 mm
0.0050 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 20 g/10 min
@Load 5.00 kg,
Temperature 300 °C
20 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM D785
Tensile Strength at Break 112 MPa16200 psi5 mm/min; ASTM D638
 112 MPa16200 psi5 mm/min; ISO 527
Elongation at Break 2.7 %2.7 %5 mm/min; ISO 527
 2.9 %2.9 %5 mm/min; ASTM D638
Tensile Modulus 5.40 GPa783 ksi5 mm/min; ASTM D638
 5.60 GPa812 ksi1 mm/min; ISO 527
Flexural Strength 163 MPa23600 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 163 MPa23600 psiyield, 2 mm/min; ISO 178
Flexural Modulus 5.20 GPa754 ksi1.3 mm/min, 50 mm span; ASTM D790
 5.20 GPa754 ksi2 mm/min; ISO 178
Izod Impact Notched 72.0 J53.1 ft-lbASTM D256
 61.0 J
@Temperature -30.0 °C
45.0 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 5.00 J/cm9.37 ft-lb/inASTM D4812
 5.00 J/cm
@Temperature -30.0 °C
9.37 ft-lb/in
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 27.0 kJ/m²12.8 ft-lb/in²80*10*4; ISO 180/1U
 28.0 kJ/m²
@Temperature -30.0 °C
13.3 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 10.0 J7.38 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
19.4 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 64.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
35.6 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °C311 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 153 °C
@Thickness 3.20 mm
307 °F
@Thickness 0.126 in
unannealed; ASTM D648
 154 °C
@Thickness 6.40 mm
309 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 161 °C322 °FRate B/50; ISO 306
 163 °C325 °FRate B/120; ISO 306
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94  V-1
@Thickness >=0.750 mm
V-1
@Thickness >=0.0295 in
UL 94
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 300 - 325 °C572 - 617 °F
Zone 2 275 - 320 °C527 - 608 °F
Zone 3 290 - 325 °C554 - 617 °F
Melt Temperature 300 - 325 °C572 - 617 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82408 / 290355

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.