MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BiologiQ BioBlend® BC 27250 Biopolymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Description:
  • One of the BioBlend® BC Biodegradable/Compostable Resins designed for films and bags.
  • Made from 50% annually renewable agricultural resources, including NuPlastiQ® CG BioPolymer (also known as the GP 1000 series), which is certified by TUV to be industrial compostable.
  • BioBlend® BC 27250 is supplied in pellet form, fully compounded and ready for film production.
Applications:
  • BioBlend® BC 27250 is intended for films and bags.
  • Used for products that require biodegradation and are intended for compost environments.

Information provided by

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D792
Melt Flow 2.9 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.9 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 12.0 MPa1740 psiASTM D638
Film Elongation at Break, MD 330 %330 %ASTM D882
Film Elongation at Break, TD <= 460 %<= 460 %ASTM D882
Elongation at Break 110 %110 %ASTM D638
Flexural Modulus 0.310 GPa45.0 ksiASTM D790
1% Secant Modulus 239 MPa34700 psiASTM D638
Elmendorf Tear Strength MD <= 380 g<= 380 gASTM D1922
Elmendorf Tear Strength TD 160 g160 gASTM D1922
Dart Drop Test 0.380 g0.000838 lbASTM D1709
Film Tensile Strength at Break, MD 21.4 MPa3100 psiASTM D882
Film Tensile Strength at Break, TD 19.13 MPa2775 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 140 - 160 °C284 - 320 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Drying Temperature 60.0 °C
@Time 3600 - 14400 sec
140 °F
@Time 1.00 - 4.00 hour
warm, dry air
Moisture Content <= 0.50 %<= 0.50 %ASTM D6980

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBIOLQ515 / 250875

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.