MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Taiwan PU CPU-105-P290B Polyurethane Shoe Mold System
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Key features:
  • Mixing ratio: 10:1
  • High bonding strength
  • Working time 30-40 mins
  • Curing time 12-16 hours
  • Excellent water and weather resistance
  • Suitable to bond with varied materials
Application:
  • Adhesion and repair of PU rubber mold
  • Wall and floor tile adhesive for partition of bathroom, kitchen…etc.
  • Adhesion for metal, wood, glass, and concrete…etc.
  • Sealing of calcium silicate board…etc
Product Introduction: CPU-49-91J is a urethane-modified-epoxy-based two-component adhesive. It can be used as PU rubber mold repair adhesive. Moreover, CPU-49-91J demonstrates excellent bonding, water, and weather resistance properties, perfect for wall and floor tile adhesion to fix almost all tiles in many challenging environments. CPU-49-91J can be applied to various surfaces such as metal, glazed tiles, and timber as well.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 2000 - 3000 cP2000 - 3000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 88 - 9288 - 92
 
Processing PropertiesMetricEnglishComments
Pot Life 10.0 - 15.0 min
@Load 0.0500 kg
10.0 - 15.0 min
@Load 0.110 lb
 
Descriptive Properties
AppearanceLight yellow elastomerAppearance of final product
Mixing ratio1:1Mixing ratio by weight with CPU-105-M309A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU057 / 305787

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.