MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TTC Taita TAITALAC® 6000 ABS, Impact Modified
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Characteristics:
  • Injection
  • High impact
  • Good flow for process
Applications:
  • Office equipment
  • OA product
  • Low temperature use
  • Shoes

Information provided by Taita Chemical Company, Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccISO 1183
Moisture Absorption at Equilibrium <= 0.30 %<= 0.30 %C/50% RH; ISO 62
Linear Mold Shrinkage <= 0.0040 cm/cm<= 0.0040 in/in60×60×2mm Sflow; ISO 294-4
Melt Flow 12 g/10 min
@Load 10.0 kg,
Temperature 220 °C
12 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103ISO 2039-2
Tensile Strength at Break 30.0 MPa4350 psi50 mm/min; ISO 527
Tensile Strength, Yield 40.0 MPa5800 psi50 mm/min; ISO 527
Elongation at Break 30 %30 %50 mm/min; ISO 527
Flexural Yield Strength 61.0 MPa8850 psi2.0 mm/min; ISO 178
Flexural Modulus 1.70 GPa247 ksi2.0 mm/min; ISO 178
Izod Impact, Notched (ISO) 27.0 kJ/m²12.8 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 2.80 J/cm²13.3 ft-lb/in²ISO 179/1A
 
Electrical PropertiesMetricEnglishComments
Hot Wire Ignition, HWI 17 sec
@Thickness <=1.57 mm
17 sec
@Thickness <=0.0620 in
UL-746A
High Amp Arc Ignition, HAI 200 arcs
@Thickness <=1.57 mm
200 arcs
@Thickness <=0.0620 in
UL-746A
High Voltage Arc-Tracking Rate, HVTR 0.000 mm/min
@Thickness <=1.57 mm
0.000 in/min
@Thickness <=0.0620 in
UL-746A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °Funannealing; ISO 75
Vicat Softening Point 100 °C
@Load 1.00 kg
212 °F
@Load 2.20 lb
50°C/hr; ISO 306
UL RTI, Electrical 60.0 °C
@Thickness <=1.57 mm
140 °F
@Thickness <=0.0620 in
UL-746B
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTTC004 / 281524

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.