MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Cosmic Plastics FARBOSET® 9020 Epoxy Powder
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Cosmic FARBOSET 9020 is a nonanhydride epoxy powder coating featuring excellent moisture resistance.

Applications: This compound is ideally suited for both radial and axial components such as ceramic and film capacitors, coils, thermistors and resistors. It can be applied using fluidized bed, wheel coaters, or electrostatic spray techniques.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccMolded
Water Absorption 0.100 %
@Time 86400 sec
Particle Mesh Size <= 80.0 Mesh1%
 325 Mesh27-33%
Storage Temperature 18.0 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.2
@Frequency 1000 Hz
ASTM 150
Dielectric Strength 900 V/milASTM 149
Dissipation Factor 0.00600
@Frequency 1000 Hz
ASTM 150
Dielectric Loss Index 0.0250
@Frequency 1000 Hz
ASTM 150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
Glass Transition Temp, Tg 125 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 min
@Temperature 160 °C
 30.0 min
@Temperature 150 °C
 60.0 min
@Temperature 130 °C
Gel Time 0.967 min
@Temperature 150 °C
Hot Plate
Shelf Life 4.00 Month
@Temperature 21.0 °C
 12.0 Month
@Temperature 4.00 °C
 
Descriptive Properties
Application and Cure Range125 – 175°C
Edge Coverage40%ASTM D-2967
Plate Flow36 mm150°C (302°F) / 60° angle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOSM033a / 325079

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.