MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe Lescalloy® AF 1410 VIM-VAR ; 13.5 in High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical, fracture-sensitive aerospace structural applications. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide superior cleanliness, ingot homogeneity, and to enhance mechanical properties.

Heat Treatment - 857°C - 1 hour oil quench; -73°C - 1 hr air warm; 510°C - 5 hrs air cool

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.283 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 242 ksiTransverse
 242 ksiLongitudinal
Tensile Strength, Yield 1517 MPaTransverse
 1531 MPaLongitudinal
Elongation at Break 16 %Longitudinal
 16 %Transverse
Reduction of Area 66 %Transverse
 71 %Longitudinal
Modulus of Elasticity 29400 ksi
Charpy Impact 68.0 JV-Notch, Transverse
 75.0 JV-Notch, Longitudinal
 
Processing PropertiesOriginal ValueComments
Processing Temperature 168 °CMartensitic Finish
 336 °CMartensitic Start
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.15 %
Chromium, Cr 2.0 %
Cobalt, Co 14 %
Iron, Fe 72.65 %
Manganese, Mn 0.10 %
Molybdenum, Mo 1.0 %
Nickel, Ni 10 %
Silicon, Si 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe Lescalloy® AF 1410 VIM-VAR ; 17 in High Strength Alloy Steel
Carpenter AerMet® 100 Aged at 875°F
AF1410 High Fracture-Toughness Steel
AISI Grade 18Ni (250) Maraging Steel, 3.18 mm thick sheet, solution annealed at 815°C (1500°F) for 30 minutes, air cooled, aged at 480°C (900°F) for 3 hours
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition A

NTIMK030 / 19378

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.