MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M FG7-22 FB-700 Filter Bag Fabric
Categories: Other Engineering Material

Material Notes: 3M has developed a line of advanced textiles for manufacturing high temperature filter bags which can be used at temperatures up to 700°F (371°C), or for those even higher temperature applications up to 900°F (482°C). These advanced fabrics have proven successful in hot gas filtration bag houses. (Typical properties of the textiles are provided on back.)

Features:

  • Efficient particulate filtration
  • High temperature capability
  • Resistance to thermal excursions
  • Abrasion resistance
  • Retrofit existing baghouses
Applications:
  • Cement
  • Incineration
  • Chemical processing
  • Petrochemical
  • Product collection
  • Coal-fired boilers

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Permeability 20 - 4020 - 40[ft3/ft2.min], @ H2O, Air w/o sizing
 
Mechanical PropertiesMetricEnglishComments
Tear Strength 35.0 kN/m200 pliwarp
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 371 °C700 °Fcontinuous operation
 427 °C801 °Fshort excursions

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33031 / 167778

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.