MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Daplen™ EE189HP Polypropylene, Mineral Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Daplen™ EE189HP is a mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and is easy to process.

Special Features:

  • High scratch resistance
  • No tendency to show stickiness after outdoor exposure
Applications: Daplen EE189HP has been developed especially for the car industry to be used in automotive interior parts:
  • Door panels and pockets
  • Center consoles
  • Window frames
  • Other automotive interior parts
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
Melt Flow 13.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
13.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 21.0 MPa3050 psi50 mm/min; ISO 527-2
Flexural Modulus 1.75 GPa254 ksi2 mm/min; ISO 178
Charpy Impact, Notched  0.400 J/cm²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C201 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 80.0 °C104 - 176 °F
 210 - 250 °C410 - 482 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
 
Descriptive Properties
Emission< 40 µg C/gVDA 277
Flow front speed100 - 200 mm/s
Fogging<1,5mg100 °C,16 h; DIN 75201

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9687 / 323044

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.