MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Pyrotek Ceramite® INS Refractory
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Ceramite® INS is a cast refractory using a bauxite based material, providing properties of electrical insulation, high mechanical strength and wear resistance. The aggregates in this formulation have a maximum grain size of approximately 4 millimeters (0.16 inches) and the castings have a maximum service temperature of 1000°C (1832°F). Ceramite INS blocks have passed Nemko electrical insulation testing under the application of 500 volts direct current and up to 5000 volts alternating current with no flash-over.

Benefits:

  • Excellent electrical insulation
  • Good mechanical strength
  • Good wear resistance
Applications:
  • Crust breaker insulators
  • Electrical insulation between steel pipes in potrooms

Information provided by Pyrotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  2.80 g/cc
@Temperature 20.0 °C
0.101 lb/in³
@Temperature 68.0 °F
 2.80 g/cc
@Temperature 600 °C
0.101 lb/in³
@Temperature 1110 °F
Grain Size <= 4000 µm<= 4000 µm
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.0150 GPa
@Temperature 20.0 °C
2.18 ksi
@Temperature 68.0 °F
Cold
 0.0200 GPa
@Temperature 850 °C
2.90 ksi
@Temperature 1560 °F
Cold
 0.0250 GPa
@Temperature 500 °C
3.63 ksi
@Temperature 932 °F
Cold
 0.0300 GPa
@Temperature 600 °C
4.35 ksi
@Temperature 1110 °F
Cold
Compressive Strength  145 MPa
@Temperature 20.0 °C
21000 psi
@Temperature 68.0 °F
Cold
 150 MPa
@Temperature 850 °C
21800 psi
@Temperature 1560 °F
Cold
 215 MPa
@Temperature 500 °C
31200 psi
@Temperature 932 °F
Cold
 230 MPa
@Temperature 600 °C
33400 psi
@Temperature 1110 °F
Cold
Abrasion  4.0
@Temperature 20.0 °C
4.0
@Temperature 68.0 °F
[cm^3]
 4.0
@Temperature 600 °C
4.0
@Temperature 1110 °F
[cm^3]
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  2.50 W/m-K
@Temperature 900 °C
17.4 BTU-in/hr-ft²-°F
@Temperature 1650 °F
 2.70 W/m-K
@Temperature 600 °C
18.7 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 3.20 W/m-K
@Temperature 300 °C
22.2 BTU-in/hr-ft²-°F
@Temperature 572 °F
Maximum Service Temperature, Air 1000 °C1830 °F
Shrinkage -0.600 %
@Temperature 20.0 - 850 °C
-0.600 %
@Temperature 68.0 - 1560 °F
 
Descriptive Properties
Permanent Linear Change-0.3%20-850°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CPYRO518 / 199540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.