MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Chemical Concepts ChemSet™ Ultralok 300 Structural Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: UltraLok™ is a two-part methacrylate, structural bonding adhesive designed for the structural bonding of various substrates, including fiberglass, steel, aluminum, and various plastics (not low energy surfaces). With a mix ratio of 1:1, UltraLok has a working time of 3 to 6 minutes and achieves nearly 90 percent of its ultimate strength in 10 to 15 minutes at room temperature curing. UltraLok provides high strength bonds to the above reference surfaces with generally no preparation effort. UltraLok bonds very strongly to steel, stainless steel, and aluminum metals. UltraLok adhesives are NOT UV STABLE, AND WILL YELLOW OVER TIME. This yellowing will not affect bond performance. Excellent Resistance to: hydrocarbons, acids and bases, vinegar, wine and condiments, most household foods. Susceptible to: polar solvents, super strong acids and bases.

UltraLok resin (Part A) and activator (Part B) are flammable. Contents include Methacrylate ester and acids. Keep containers closed after use. Wear gloves and safety glasses to avoid skin and eye contact. Wash with soap and water after skin contact. In case of eye contact, flush with water for 15 minutes and get medical attention. Harmful if swallowed. Keep out of the reach of children. Keep away from heat, sparks, and open flames. To assure maximum bond strength, surfaces must be mated together within the specified working time, and all clamps affixed within that time. Use sufficient material to ensure that the joint is completely filled when parts are mated and clamped. Avoid over clamping parts, which may cause a dry joint or a joint starved of adhesive. All adhesive application, part positioning, fixturing, and clamping should occur before the working time of the adhesive has expired. After the indicated working time, parts must remain undisturbed until the fixture time is completed. Components bonded, adhesive, and shop temperature can have a significant effect on the work and fixture time of the adhesive. Application of UltraLok adhesive at temperatures between 65°F and 85°F (18°C and 30°C) will ensure proper cure. Temperatures below 65°F (18°C) will slow cure and fixture speed. UltraLok adhesives will still react, but will take longer. Temperatures above 85°F (18°C and 30°C) will increase cure and fixture speeds, and there’s a risk that the adhesive will be hardened or too thick to bond materials. The viscosities of UltraLok adhesives are affected by temperature. Because of the curing features of UltraLok adhesives, large amounts of heat are generated when large masses of material are mixed at one time. The heat generated by the exotherm resulting from mixing large amounts of adhesive can result in a boiling of the monomer in the adhesive (methyl methacrylate), resulting in the release of trapped air, steam and volatile gasses. To prevent this, use only enough material as needed for use within the working time for the product, and confine the gap or spread out the material to no more than .50 inches.

The shelf life of UltraLok is twelve (12) months from the date of manufacture based upon continuous storage at room temperature. Storage of UltraLok adhesives in refrigerated compartments will extend the shelf life even more. Do not store UltraLok adhesive or any other adhesives in a refrigerator which has food or lunch products in them. Bring UltraLok adhesives to room temperature for 24 hours before use, otherwise longer cure and fixture times may be expected. Long-term storage at temperatures above room temperature will shorten the shelf life of UltraLok adhesives considerably. Storage at temperatures above 100°F or 38°C could shorten the shelf life to less than one month. UltraLok adhesives contain no water, so freezing of the adhesive for short periods is permissible, but is not encouraged.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³activator, uncured
 0.971 g/cc0.0351 lb/in³mixed
 0.983 g/cc0.0355 lb/in³resin, uncured
Viscosity 40000 - 90000 cP40000 - 90000 cPuncured, resin
 100000 - 150000 cP100000 - 150000 cPuncured, activator
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength >= 6.89 MPa>= 1000 psiSubstrate: ABS/PVC sheeting. Failure type: substrate.; ASTM D638
 >= 17.2 MPa>= 2500 psiSubstrate: Fiberglass surface. Failure type: substrate.; ASTM D638
 17.2 - 24.1 MPa2500 - 3500 psiSubstrate: steel/stainless steel. Failure: cohesive.; ASTM D638
 17.2 - 24.1 MPa2500 - 3500 psiSubstrate: aluminum. Failure: cohesive.; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Flash Point 10.6 °C51.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 18.3 - 29.4 °C65.0 - 85.0 °F
Working Life 3.00 - 6.00 min
@Temperature 23.0 °C
3.00 - 6.00 min
@Temperature 73.4 °F
 
Descriptive Properties
Coloramber, activator, uncured
 translucent, resin, uncured
Fixture Time10 to 15 minutes at 75°F. Room temperature cure.
Gap Filling0.375 inches
Mix Ratioresin 1.0: activator 1.0 (wt or vol)
Time before moving18 to 24 minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEMI906 / 232145

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.