MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 1.0 PHR Zinc Stearate
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators..

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 65>= 65
Tensile Strength 29.30 MPa4249 psi
Elongation at Break 565 %565 %
100% Modulus 2.70 MPa
@Strain 100 %
392 psi
@Strain 100 %
200% Modulus 5.80 MPa
@Strain 200 %
841 psi
@Strain 200 %
300% Modulus 9.701 MPa
@Strain 300 %
1407 psi
@Strain 300 %
Tear Strength 34.6 kN/m197 pliDie C
Compression Set 31.7 %
@Temperature 70.0 °C,
Time 79200 sec
31.7 %
@Temperature 158 °F,
Time 22.0 hour
 
Processing PropertiesMetricEnglishComments
Cure Time 9.50 min
@Temperature 155 °C
0.158 hour
@Temperature 311 °F
 
Descriptive Properties
Formulation as Tested1Thanecure® ZM
 1Zinc Stearate
 1.5Sulfur
 10Cumar P10
 100Millathane E34
 2MBT
 30N330 Black
 4MBTS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMILL404 / 87448

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.