MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

EOS CopperAlloy CuCrZr DMSL on EOS M 400; 80 µm Layer Thickness
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Copper Alloy

Material Notes: Copper alloy CuCrZr has a favorable combination of electrical and thermal conductivity accompanied with good mechanical properties. This alloy reaches its good properties during heat treatment.

Main Characteristics:

  • High productivity 12 mm3/s with 80 µm layer thickness
  • Moderate to high conductivity in heat treated condition together with good mechanical properties
  • Chemical composition corresponds to C18150 and CW106C
Typical Applications:
  • Rocket engine parts
  • Heat exchangers
  • Induction coils
heat-treatment: 1. Hold 30 min at ~ 980 °C in argon atmosphere, water cooling to room temperature. 2. Hold 3 h at ~ 430 °C in argon atmosphere, slow cooling in argon by taking the samples out of the furnace and rest in air.

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Porosity <= 0.50 %<= 0.50 %
Thickness 80.0 microns3.15 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 210 MPa30500 psias manufactured
 300 MPa43500 psiheat treated
Tensile Strength, Yield 160 MPa23200 psias manufactured
 200 MPa29000 psiheat treated
Elongation at Break 30 %30 %heat treated
 40 %40 %as manufactured
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0000020 ohm-cm<= 0.0000020 ohm-cmHeat-treated; ASTM E1004-17
 <= 0.0000086 ohm-cm<= 0.0000086 ohm-cmas manufactured & heat treated, IACS (ASTM E1004-17); ASTM E1004-17
 
Descriptive Properties
Volume rate12 mm3/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS928 / 280588

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.