MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Konson TDEC Rubber Accelerator
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: Tellurium Diethyl Dithiocarbamate

Molecular Formula: C20H40N4S8 Te

CAS#: 20941-65-5

Properties: Density (on 20?) is 1.48 g/cm3. The loosen density is approx 0.32~0.36 g/cm3. Soluble in chloroform, benzene, and carbon disulfide, slightly soluble in alcohol and gasoline, insoluble in water.

Applications: As a kind of super accelerator used to natural rubber, styrene-butadiene rubber. Commonly, using with some other kind of accelerators such as benzothiazole, sulfenamide. A fast velocity at vulcanizing temperature can be obtained, and in tensile can be increased. Suitable for making inner tube of tires, soft tube, isolating layer of wire and cable, etc.. Don’t use for manufacturing the products contacting with foods. TDEC is regulated for use in articles in contact with food as specified under BgVV XXI, Category 4.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³
Molecular Weight 721 g/mol721 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 108 °C>= 226 °FInitial
 
Descriptive Properties
AppearanceLight-orange to yellow powder
Content16.5-19%Tellurium
Heat Loss<0.5%
Sieve residue<0.1%150µm
 <0.5%63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS048 / 256093

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.