MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Nextel™ CF-40 Woven Fabric 550
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.03 g/cc0.109 lb/in³
Permeability 3535[ft3/min/ft2], Air w/o sizing
Thickness 940 microns37.0 mil
Fiber Count 2220 dtex2000 denier1/2
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 2000 MPa290000 psifilament 25.4mm
Tensile Modulus 193 GPa28000 ksifilament
Tear Strength 45.1 kN/m258 pliFill, Breaking Strength w/o Sizing
 59.8 kN/m342 pliWarp, Breaking Strength w/o Sizing
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.8
@Frequency 9.375e+9 Hz
5.8
@Frequency 9.375e+9 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.30 µm/m-°C
@Temperature 100 - 1100 °C
2.94 µin/in-°F
@Temperature 212 - 2010 °F
Melting Point 1800 °C3270 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.6021.602
 
Component Elements PropertiesMetricEnglishComments
Al2O3 73 %73 %
SiO2 27 %27 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Griltech Grilon® TM 5000 White Nylon 6 Fiber
Akro-Plastic Akrotek® PK-VM GF 60 (4923) PK Dry, 60% Glass Filled
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Conditioned, 60% Glass Filled

PMM33018 / 167765

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.