MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: High tensile strength, low temperature flexibility, and high adhesion to various substrates such as PET, PVC, and various fabrics.

Uses: Fabric coating and audio tape binder, inks and solution cast pigment dispersion media

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Brookfield Viscosity 200 cP200 cPRVT Spindle #2, 20 RPM, 23°C, 15% T.S. in MEK
 1500 cP1500 cPRVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength 50.3 MPa7300 psiASTM D412/D638
Elongation at Break 430 %430 %ASTM D412/D638
100% Modulus 2.30 MPa
@Strain 100 %
334 psi
@Strain 100 %
ASTM D412/D638
300% Modulus 5.90 MPa
@Strain 300 %
856 psi
@Strain 300 %
ASTM D412/D638
Peel Strength 0.260 kN/m1.48 pliAdhesion to PET; TP-141
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 35.0 °C95.0 °FASTM D1525
Glass Transition Temp, Tg 19.0 °C66.2 °FDSC

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5708 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane

PNOVEON017 / 55282

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.