MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture
Categories: Polymer

Material Notes: Features/Benefits:
  • Outlasts silicone tubing in peristaltic pumps by up to 30 times
  • Low particulate spallation
  • Can be autoclaved repeatedly
  • Temperature resistant from -60°F to 275°F
  • Withstands repeated CIP and SIP cleaning and sterilization
  • Fully tested to ISO 10993 standards to facilitate validation process
  • Meets USP Class VI FDA and NSF criteria
Typical Applications include: Diagnostic test product manufacturing, cell harvest and media process systems, vaccine manufacturing, bioreactor process lines, production filtration and fermentation, sterile filling, shear sensitive fluid transfer.
UL94-HB Flame Resistance Classification Passed. All data based on a 0.0625 inch test sample.(Available in multiple thicknesses.)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccASTM D792-91
Water Absorption 0.30 %24 hours at 23°C; ASTM D570-81
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 64Value given for 15 second test.; ASTM D2240-91
Tensile Strength, Yield 1000 psiASTM D-412-92
Tensile Stress at Strain 410 psi
@Strain 100 %
ASTM D412-92
Elongation at Break 375 %ASTM D-412-92
Tear Strength 120 pliTear Resistance; ASTM D1004-93
Compression Set 27 %
@Temperature 70.0 °C,
Time 79200 sec
Constant Deflection; ASTM D395-89 Method B
Tensile Set 47 %at 75% Elongation; ASTM D412-92
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 535 V/milASTM D149-93
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 275 °FValue given for heat resistance, not necessarily a recommended operating temperature.
Brittleness Temperature -75.0 °FASTM D746-79
 -40.0 °FLow Temperature Flexibility; ASTM D412-92
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation
Saint-Gobain Tygon® A-60-F Food Process Tubing Formulation
Saint-Gobain Tygon® Noroprene® Chemical Tubing Formulation
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing

PSTGQZ507 / 69021

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.