Treatment required for max strength: as supplied Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman. Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011. |
ASTM B-196, QQ-C-530, AMS 4533, 4534, 4650 & 4651, RWMA Class 4 |