General purpose, 75°C rated non-lead stabilized jacket compound with good low temperature properties and 720 hour sunlight resistance. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |