Description: TATREN HT 25 11 is a controlled rheology homopolymer of very narrow molecular weight distribution. Consistent quality, good color and thermal stability. This grade contains anti gas fading additive package. Applications: TATREN HT 25 11 is suitable for injection molding of general purpose items, extrusion coating of PP fabrics and for compounding. TATREN HT 25 11 can be used also for undemanding textile applications. (1) Typical properties measured on standard injection molded test specimen according to ISO 294-1. Information provided by Molgroup Chemicals |