MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC SABIC® PP 108CS20 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound 108CS20 is a material with good flow, impact and stiffness. The material is part of the SABIC® PP CS systems and also available as a CS system: using a mixture of 60% SABIC® PP 108MF10 and 40% SABIC® PPcompound 20MBT yields similar properties as listed below. SABIC® PPcompound 108CS20 is a designated automotive grade. IMDS ID: 111851732

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccInjection molded sample ISO527-1A; ISO 1183
Filler Content 20 %SABIC method
Linear Mold Shrinkage 0.0090 cm/cmInjection molded plaque 65x65x3.2mm; SABIC method
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ISO 868
Tensile Strength at Break 17.0 MPaISO 527/1A
Tensile Strength, Yield 20.0 MPaISO 527/1A
Elongation at Break 100 %ISO 527/1A
Tensile Modulus 1500 MPaISO 527/1A
Flexural Modulus 1500 MPaISO 178/1A
Izod Impact, Notched (ISO) NBISO 180/1A
 7.00 kJ/m²
@Temperature -20.0 °C
N.B.: No Break; ISO 180/1A
 25.0 kJ/m²
@Temperature 0.000 °C
N.B.: No Break; ISO 180/1A
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched NBISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
 80.0 µm/m-°C
@Temperature -30.0 - 100 °C
ISO 11359-2
 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 110 °CISO 75
Vicat Softening Point 130 °Cat 10 N (VST/A); ISO 306/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11382 / 244849

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.