MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Kalix® 2930 HFFR High Performance (HPPA), Bio-sourced
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: Bio-sourced, meets UL 94V2 at 0.4 mm for electronic devices

Kalix® 2930 HFFR is a bio-sourced polyamide-based material specifically formulated to meet UL 94V2 @ 0.4 mm requirements for electronic devices. The material uses an advanced halogen-free flame retardant package expressly designed to minimize blooming, plate out, and other process related issues commonly associated with flame retardant materials.

- Black: Kalix® 2930 HFFR BK 000

Applications: Cell Phones; Electrical Parts; Electrical/Electronic Applications; Thin-walled Parts

Features: Fast Molding Cycle; Flame Retardant; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Low Warpage; Paintable; Platable

- Typical values shown tested on Dry as Molded samples.

- Standard Packaging and Labeling: Kalix® HFFR resin is packaged in foil lined, multiwall paper bags containing 25 kg (55 pounds) of material. Individual packages will be plainly marked with the pr

Injection notes: Storage:
- Kalix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Kalix® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Kalix® processing guide.
Drying:
- Kalix® compounds are supplied in sealed bags. It should be dried before molding because excessive moisture content will result in reduced mechanical properties and processing issues, such as excessive nozzle drooling, foaming and splay visible on the molded parts.
- Drying temperatures of up to 100°C may be used for dark colored resin (such as black) to achieve shorter drying times, if necessary. For lighter colored resin, 80°C drying temperature is recommended to minimize the risk of oxidative discoloring.
- Use of a desiccant dryer with -40°C dewpoint is strongly suggested to ensure Kalix® material has reached optimum moisture content before processing.
Injection Molding:
- Set injection pressure to give rapid injection. Adjust holding pressure to one-half injection pressure. Set hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled.
Tooling:
- This material is not typically recommended for use in hot runner systems due to the possibility of tooling corrosion and wear. If hot runner systems must be used please engage a tooling vendor having adequate experience with flame-retardant, glass-filled polyamides. Ensure that appropriate corrosion-resistant and wear-resistant tool steels and coatings are utilized to increase tooling life cycles.
- Excessive pellet moisture, melt temperature, residence times will accelerate the possibility of corrosion. It is critical that recommended processing parameters are followed to minimize corrosion potential.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/cc
Water Absorption 0.17 %
@Time 86400 sec
0.17 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress 130 MPa18900 psiISO 527-2
Elongation at Break 2.4 %2.4 %ISO 527-2
Tensile Modulus 10.6 GPa1540 ksiISO 527-2
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 55.0 kJ/m²26.2 ft-lb/in²ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °F
Deflection Temperature at 1.8 MPa (264 psi) 206 °C403 °FUnannealed; ISO 75-2/A
Glass Transition Temp, Tg 65.0 °C149 °FDSC
Flammability, UL94 V-2
@Thickness 0.400 mm
V-2
@Thickness 0.0157 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 255 - 265 °C491 - 509 °F
Front Barrel Temperature 265 - 280 °C509 - 536 °F
Melt Temperature 260 - 300 °C500 - 572 °FInjection
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 - 100 °C
@Time 14400 - 43200 sec
176 - 212 °F
@Time 4.00 - 12.0 hour
Moisture Content <= 0.070 %<= 0.070 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding; Water-Heated Mold Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4302 / 280102

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.