Hostacom TRC 483N NA KX8A DKSLTE is a high flow, mineral-filled UV stabilized thermoplastic elastomeric olefin (TEO) resin with excellent balance of processability, rigidity, impact and scratch/mar resistance that is typically used for interior trim and door panel applications. Availability: North America Application: Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Excellent Processability; High Impact Resistance; High Rigidity; Scratch Resistant; UV Stabilized Information provided by LyondellBasell. |