MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ampco Metal AMPCO® 18 Aluminum Bronze, Rectangular
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Compact grain structure and high physical properties result from proper phase distribution and hot working of AMPCO 18 during the extrusion process. These qualities enable this alloy to perform successfully in an extremely wide range of difficult applications. It is an excellent bearing material characterized by good resistance to wear and fatigue.

Applications: AMPCO 18 rod is produced with a good surface finish to commercial tolerances and can be used economically for volume-production applications. AMPCO 18 is ideally suited where high strength and hardness combined with wear and fatigue resistance are required. Some of the more common applications of this alloy are bushings, bearings, gears, worm wheels, valve seats and guides, hydraulic valve parts, pump rods, guide pin bushings, gibs and slides, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.45 g/cc0.269 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 192192HB 30
Hardness, Rockwell B 9292
Tensile Strength, Ultimate 689 MPa99900 psi
Tensile Strength, Yield 351 MPa
@Strain 0.5 %
50900 psi
@Strain 0.5 %
Elongation at Break 14 %14 %
Reduction of Area 12 %12 %
Modulus of Elasticity 117 GPa17000 ksi
Compressive Yield Strength 234 MPa33900 psiProportional Limit
Compressive Strength 980 MPa142000 psi
Fatigue Strength 248 MPa
@# of Cycles 1.00e+8
36000 psi
@# of Cycles 1.00e+8
Shear Strength 428 MPa62100 psi
Izod Impact 20.0 J14.8 ft-lb
Charpy Impact 13.0 J9.59 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000142 ohm-cm0.0000142 ohm-cm12% I.A.C.S.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 °C
9.00 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity 63.0 W/m-K437 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 10.5 %10.5 %
Copper, Cu 85.5 - 86 %85.5 - 86 %As Balance
Iron, Fe 3.5 %3.5 %
Other, total <= 0.50 %<= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ampco Metal AMPCO® 18 Aluminum Bronze, Extruded and Drawn Rods, ≤ 12.7 mm.
Ampco Metal AMPCO® 25 Extruded Bar
Ampco Metal AMPCO® 18 Aluminum Bronze, Extruded and Drawn Rods, 25.4 - 76.2 mm.
Ampco Metal AMPCOLOY® 35 Tin Bronze, Continuous Cast
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C

NAMPCO11 / 14965

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.