MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Armstrong A-1/E Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°F

Information provided by Ellsworth Adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 400000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
Tensile Strength, Ultimate 5600 psiafter optimum cure
Elongation at Break 1.4 %
Adhesive Bond Strength 5900 psiSteel-Steel; after optimum cure
 2650 psi
@Temperature -54.4 °C
Aluminum-Aluminum tensile shear
 2800 psi
@Temperature 25.0 °C
Aluminum-Aluminum tensile shear
 2800 psi
@Temperature 82.2 °C
Aluminum-Aluminum tensile shear
 
Thermal PropertiesOriginal ValueComments
CTE, linear 24.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 250 °F
Glass Transition Temp, Tg 111 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 °FOptimum cure is 1 hr. @ 200°F
Pot Life 120 - 180 min
@Temperature 25.0 °C
100 g
 
Descriptive Properties
ColorBrown
Mix Ratio100/6By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP1330LV Heat Cure Epoxy Polymer System
Resin Technology Group TIGA 901 Room Temperature Curing Silver Conductive Epoxy
NextGen Adhesives TC907-33 Thermally Conductive Adhesive
Lord Adhesives Circalok™ 6037 Epoxy Adhesive
Henkel Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill

PARM01 / 24533

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.