MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wacker Elastosil® LR 6290 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® LR 6290 A/B Liquid Silicone Rubber is a two-component, solventless liquid silicone rubber system that cures rapidly upon heating to a tough silicone rubber. It has been formulated primarily for use as a heat protective, low durometer fabric coating.

Special features:

  • 100% solids
  • Good adhesion
  • Non-blocking without powder
  • Good fire retardancy
Application: Cure is accomplished by simply mixing equal parts (1:1) by weight of part A and part B. Oven cure at 172 C-200°C (340 F-392°F) for one to six minutes depending on oven, coating thickness and type of fabric used. Curing may be retarded and prevented by: nitrogen compounds such as amines and amides, sulfur compounds, anti-aging additives and other additives in rubbers and plastics, etc. Therefore, a materials compatibility test is always recommended.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/cccured; ASTM D412
Viscosity 70000 cPComponent B; ASTM D412
 82000 cPcatalyzed; ASTM D412
 92000 cPComponent A; ASTM D412
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25cured; ASTM D2240
Tensile Strength at Break >= 3.45 MPacured; ASTM D412
Elongation at Break >= 400 %cured; ASTM D412
Tear Strength >= 40.0 kN/mcured; ASTM 624 B
 
Processing PropertiesOriginal ValueComments
Pot Life 2880 min
 
Descriptive Properties
AppearancetranslucentComponent B
 whiteComponent A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9173 / 204702

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.