MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese VECTRA E480i LCP, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled

Material Notes: Easy flowing grade with very good heat resistance and mechanical properties with reduced warpage.
VECTRA should in principle be predried. Because of the necessary low maximum residual moisture content the use of dry air dryers is recommended. The dew point should be =< - 40° C. The time between drying and processing should be as short as possible.
For subsequent storage of the material in the dryer until processed the temperature does not need to be lowered for grades A, B, C, D and V (<= 24 h).

Information provided by Celanese Corporation.

Key Words: Glass reinforced variant with high flow and reduced warpage. Suitable for lead free solder.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Linear Mold Shrinkage, Flow 0.00 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPa5mm/min; ISO 527-2/1A
Elongation at Break 1.2 %5mm/min; ISO 527-2/1A
Tensile Modulus 17000 MPa1mm/min; ISO 527-2/1A
Flexural Strength 200 MPaISO 178
Flexural Modulus 17000 MPaISO 178
Flexural Strain at Break 1.8 %ISO 178
Izod Impact, Notched (ISO) 28.0 kJ/m²ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 335 °CISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 270 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 30.0 °Chopper
 80.0 - 120 °Ccavity
Feed Temperature 60.0 - 80.0 °C
Zone 1 315 - 325 °C
Zone 2 320 - 330 °C
Zone 3 325 - 335 °C
Zone 4 330 - 340 °C
Die Temperature 335 - 345 °C
Melt Temperature 335 - 345 °C
Drying Temperature 150 - 170 °C
Dry Time 4 - 6 hour
Moisture Content 0.010 %Necessary low maximum
Injection Pressure 7250 - 21750 psi
Hold Pressure 7250 - 21750 psi
Back Pressure <= 435 psi
Screw Speed 80 rpm
@Diameter 40.0 mm
 140 rpm
@Diameter 25.0 mm
 200 rpm
@Diameter 16.0 mm
Hot-Working Temperature 335 - 345 °C
 
Descriptive Properties
Injection speedvery fast
RemarksWhen using short metering strokes an accumulator is recommended to get short injection times.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 101L BKB080 PA66
Celanese Vectra® C550 Liquid Crystal Polymer (LCP), 50% Mineral Filled
Celanese ZENITE 17311 EFT LCP, 35% Mineral / Glass Reinforced
Aluminum, Al
Avient Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber

PHCS475 / 123890

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.