MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).

Appearance: Translucent spherical pellets

Uses: Injection molding parts

Available in Europe

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccISO 2781
Maximum Moisture Content 0.050
Melt Flow 15 - 40 g/10 min
@Load 8.70 kg,
Temperature 215 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ISO 868
Tensile Strength, Ultimate 43.0 MPaISO 37
Elongation at Break 650 %ISO 37
Tensile Modulus 0.0280 GPaISO 527
50% Modulus 0.00750 GPa
@Strain 50 %
ISO 37
100% Modulus 0.00900 GPa
@Strain 100 %
ISO 37
300% Modulus 0.0150 GPa
@Strain 300 %
ISO 37
Rebound 40 %ISO 4662
Tear Strength 85.0 kN/mwith incision; ISO 34B
 121 kN/mwithout incision; ISO 34B
Abrasion 35mm3; ISO 4649
Compression Set 23 %
@Temperature 22.0 °C,
Time 252000 sec
ISO 815
 33 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 115 °CA50; ISO 306
 
Processing PropertiesOriginal ValueComments
Feed Temperature 40.0 °CInjection
Nozzle Temperature 190 - 200 °CInjection
Zone 1 185 - 195 °CInjection
Zone 2 190 - 200 °CInjection
Zone 3 195 - 205 °CInjection
Zone 4 195 - 205 °CInjection
Drying Temperature 100 °C
Dry Time 2.00 - 3.00 hour
Dew Point -30.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane

PNOVEON161 / 55431

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.